Calcium lignosulphonate was used to synthesize a spherical lignosulphonate resin in a cheap and non-toxic disperse medium by reversed phase suspension polymerization. The process conditions were optimized by orthogonal experiments. Under the optimal conditions (T95C, cHCl3 molL1, mHCHOmCLS7%, wCLS 50%), globulation took about 20 min and the product was featured with excellent spherical shape, narrow particle size range, 61.20% of water retention capacity, 0.83 mmolml1 of total volume exchange capacity and 3.46 mmolg1 of total exchange capacity. The results of Scanning Electron Micrograph and Scanning Probe Micrograph indicate that spherical lignosulphonate resin has a rugged surface with porous microstructure in the gel skeleton. The average pore size of dry samples was determined to be 10.46 nm by the BET method